184T High Nickel Molybendum Multi-Purpose Super Alloy Stick Electrode
184 High Nickel High Strength High Corosion Resistant Tensile 110000 Polarity Dcep Elongation 30% 21Rc Heat Resistant 1800 F (5 US Pounds)
- SDS
- TAA Compliant
Welcome. Register now to see your pricing.
Close
184 High Nickel High Strength High Corosion Resistant Tensile 110000 Polarity Dcep Elongation 30% 21Rc Heat Resistant 1800 F (5 US Pounds)
A maximum-strength alloy with high nickel and molybdenum content that provides outstanding corrosion and heat resistance. Columbium alloy additions increase weld stability.
Versatile Well suited for welding Inconel 625, 706, 718 and X-750; Incoloy 800 and 825; Monel alloy K-500; Ferralium 255, Hastelloy B, C or G, and Carpenter 20 Cb and combinations of these alloys
Corrosion Resistant Highly resistant to chloride pitting and stress corrosion cracking
Excellent for dissimilar nickel alloys and nickel to ferrous alloys
Excellent for cryogenic applications
Heat resistant to 1800°F/982°C
Resists cracking when heated and cooled repeatedly
Tensile Strength: 110,000 PSI/758 MPa
Yield Strength: 95,000 PSI/655 MPa
Hardness: 21 Rc
Elevated Temperature Tensile Data: 1000°F/538°C: 85,000 PSI/586 MPa 1800°F/982°C: 25,000 PSI/172 MPa
Elongation: 30%
Impact Strength (Charpy): 48 ft.-lbs. @ -320°F/-196°C
Current: DCEP (DC+)
A maximum-strength alloy with high nickel and molybdenum content that provides outstanding corrosion and heat resistance. Columbium alloy additions increase weld stability.
Versatile Well suited for welding Inconel 625, 706, 718 and X-750; Incoloy 800 and 825; Monel alloy K-500; Ferralium 255, Hastelloy B, C or G, and Carpenter 20 Cb and combinations of these alloys
Corrosion Resistant Highly resistant to chloride pitting and stress corrosion cracking
Excellent for dissimilar nickel alloys and nickel to ferrous alloys
Excellent for cryogenic applications
Heat resistant to 1800°F/982°C
Resists cracking when heated and cooled repeatedly
Tensile Strength: 110,000 PSI/758 MPa
Yield Strength: 95,000 PSI/655 MPa
Hardness: 21 Rc
Elevated Temperature Tensile Data: 1000°F/538°C: 85,000 PSI/586 MPa 1800°F/982°C: 25,000 PSI/172 MPa
Elongation: 30%
Impact Strength (Charpy): 48 ft.-lbs. @ -320°F/-196°C