184T High Nickel Molybendum Tig Wire 3/32X36
184T High Nickel High Strength High Corosion Resistant Tensile 110000 Gas 100%Ar Elongation 30% 21Rc (5 US Pounds)
Representative Image Only
- SDS
- TAA Compliant
Welcome. Register now to see your pricing.
Close
184T High Nickel High Strength High Corosion Resistant Tensile 110000 Gas 100%Ar Elongation 30% 21Rc (5 US Pounds)
Representative Image Only
A high-strength alloy with high-nickel and molybdenum content that gives outstanding corrosion and heat resistance. It is highly resistant to chloride pitting and stress corrosion cracking. Columbium alloy additions increase weld stability. Excellent for welding dissimilar nickel base alloys and nickel alloys to ferrous metals. It is also well suited for welding Inconel 625, 706, 718 and X-750; Incoloy 800 and 825; Monel alloy K-500; Hastelloy B, C or G, and Carpenter 20 Cb.
Tensile Strength: 110,000 PSI/758 Mpa
Hardness: 21 Rc
Elevated Temperature Tensile Data: 1000°F/538°C: 85,000 PSI/507 Mpa 1800°F/982°C: 25,000 PSI/173 Mpa
Elongation: 30%
Current: DCEN (DC-)
Gas: 100% Argon
Sulfuric Acid Good up to 150°F/66°C for all concentrations, also good up to the boiling point for all concentrations below 10%
Hydrochloric Acid Very good up to 120°F/49°C for all concentrations
Nitric Acid Excellent corrosion resistance at almost all temperatures and concentrations
Phosphoric Acid Excellent at temperatures below 225°F/143°C for all concentrations
Good above 225°F/143°C, except near the boiling point in very high concentrations
Organic Acids Generally excellent at all temperatures and concentrations
Sodium Hydroxide (Caustic) Generally excellent at all temperatures and concentrations
A high-strength alloy with high-nickel and molybdenum content that gives outstanding corrosion and heat resistance. It is highly resistant to chloride pitting and stress corrosion cracking. Columbium alloy additions increase weld stability. Excellent for welding dissimilar nickel base alloys and nickel alloys to ferrous metals. It is also well suited for welding Inconel 625, 706, 718 and X-750; Incoloy 800 and 825; Monel alloy K-500; Hastelloy B, C or G, and Carpenter 20 Cb.
Tensile Strength: 110,000 PSI/758 Mpa
Hardness: 21 Rc
Elevated Temperature Tensile Data: 1000°F/538°C: 85,000 PSI/507 Mpa 1800°F/982°C: 25,000 PSI/173 Mpa
Elongation: 30%
Current: DCEN (DC-)
Gas: 100% Argon
Sulfuric Acid Good up to 150°F/66°C for all concentrations, also good up to the boiling point for all concentrations below 10%
Hydrochloric Acid Very good up to 120°F/49°C for all concentrations
Nitric Acid Excellent corrosion resistance at almost all temperatures and concentrations
Phosphoric Acid Excellent at temperatures below 225°F/143°C for all concentrations
Good above 225°F/143°C, except near the boiling point in very high concentrations
Organic Acids Generally excellent at all temperatures and concentrations